To ensure you get the best experience, this website uses cookies.
        
        
     
    
                
    
        
        
        
        
        
    
	- S11.6.7
- Test holes must be reinstated to finish flush with the surface by any of the following methods:
	
		- Using a fine aggregate bound with cement or bitumen for the upper layers as appropriate, and compacted in layers 100 mm thick, or less.
- Using a self-compacting proprietary product.
- Using a flexible sealing plug. The void beneath the flexible sealing plug must be reinstated using sand and cement mix or a proprietary product.
		
			- In bituminous surfaces, all sealing plugs must be coloured black (or dark grey).
- In modular or concrete surfaces, sealing plugs must be coloured white (or light grey) or black (or dark grey) as appropriate.
 
 
- S11.6.8
- If a flexible sealing plug becomes dislodged during the guarantee period, the undertaker must replace it.